Additional information
| Unit | Each |
|---|---|
| Style | 3C |
| Lenght | 120mm |
| Material | Superalloy |
| Points width thickness | 0.06 x 0.02mm |
€ 67,30
Lengt:120mm, Material: Superalloy, Tips:0.06 x 0.02mm
| Unit | Each |
|---|---|
| Style | 3C |
| Lenght | 120mm |
| Material | Superalloy |
| Points width thickness | 0.06 x 0.02mm |